FABRIC |
KNC 222 Super Combed Twill |
FINISH |
PERMANENT PRESS, DOUBLE PRE-SHRUNK |
FABRIC CHARACTERISTICS |
TEST METHOD |
|
|
|
BLEND |
|
65% Polyester 35% Cotton |
+ / - 3% |
|
FINISHED WEIGHT |
|
213 GSM. |
+ / - 5% |
|
YARN COUNT |
|
PT20 x PT20 |
+ / - 5% |
|
FINISHED CONSTRUCTION |
|
112 x 56 Thread/Inch |
+ / - 5% |
|
WEAVE |
|
|
Twill |
|
MINIMUM USABLE WIDTH |
|
|
59/60" |
|
PHYSICAL PERFORMANCE |
TEST METHOD |
|
|
RESULT |
TENSILE STRENGTH |
BS EN ISO 13934-2 |
|
Warp x Weft |
min 30 kg. |
SHRINKAGE IN WASHING |
BS EN ISO 6330 |
|
Length & Width |
+ / - 3% |
TEAR STRENGTH |
BS EN ISO 13937-1 |
|
Warp x Weft |
min 15 g. |
SEAM SLIPPAGE |
BS EN ISO 13936-1 |
|
Warp x Weft |
min 20 kg. |
COLOUR PERFORMANCE |
TEST METHOD |
|
|
|
RUBBING |
BS EN ISO 105x12 |
Color Staining |
Dry |
4 *** |
Color Staining |
Wet |
4 *** |
WASHING |
BS EN ISO 105 C06 |
Color Change |
|
4 *** |
Color Staining |
|
4 *** |
PERSPIRATION |
BS EN ISO 105 E04 |
Color Change |
|
4 *** |
Color Staining |
|
4 *** |
LIGHT FASTNESS |
BS EN ISO 105 B02@ STD 4 |
Color Change |
|
3-4 *** |
WATER |
BS EN ISO 105 E01 |
Color Change |
|
4 *** |
Color Staining |
|
4 *** |
SAFETY |
TEST METHOD |
|
|
|
pH |
AATCC 81 |
|
|
4.0 - 7.5 |
FORMALDEHYDE |
JIS L1041 B |
|
|
max 300 ppm |
*** : Color performance results shown are average values. Dark and Extra Dark Colors may not meet figures quoted.