FABRIC | TC 21000 | |||
FINISH | PERMANENT PRESS, DOUBLE PRE-SHRUNK | |||
FABRIC CHARACTERISTICS | TEST METHOD | |||
BLEND | 65% Polyester 35% Cotton | + / - 3% | ||
FINISHED WEIGHT | 116 GSM. | + / - 5% | ||
YARN COUNT | 45Ne x 45Ne | + / - 5% | ||
FINISHED CONSTRUCTION | 139 x 72 Thread Count/Inch | + / - 5% | ||
WEAVE | Poplin | |||
MINIMUM WIDTH | 44/45", 59/60" | |||
PHYSICAL PERFORMANCE | TEST METHOD | RESULT | ||
TENSILE STRENGTH | BS EN ISO 13934-2 | Warp x Weft | min 15 kg. | |
SHRINKAGE IN WASHING | BS EN ISO 6330 | Length & Width | + / - 3% | |
TEAR STRENGTH | BS EN ISO 13937-1 | Warp x Weft | min 700 g. | |
SEAM SLIPPAGE | BS EN ISO 13936-1 | Warp x Weft | min 8 kg. | |
COLOUR PERFORMANCE | TEST METHOD | |||
RUBBING | BS EN ISO 105 X12 | Color Staining | Dry | 4 *** |
Color Staining | Wet | 4 *** | ||
WASHING | BS EN ISO 105 C06 | Color Change | 4 *** | |
Color Staining | 4 *** | |||
PERSPIRATION | BS EN ISO 105 E04 | Color Change | 4 *** | |
Color Staining | 4 *** | |||
LIGHT FASTNESS | BS EN ISO 105 B02@ STD 4 | Color Change | 4 *** | |
WATER | BS EN ISO 105 E01 | Color Change | 4 *** | |
Color Staining | 4 *** | |||
SAFETY | TEST METHOD | |||
pH | AATCC 81 | 4.5 - 7.0 | ||
FORMALDEHYDE | JIS L1041 B | max 75 ppm. |